Styrene-Butadiene Rubber (SBR) Binder for Li-ion Battery Anode
Physical form
Milky white liquid with light blue gloss
Solidity
50±2%
PH
6-7
Viscosity (NDJ-5S, 25℃)
100~350 mPa. S
Vitrification temperature
-18 ℃
Storage Temperature
0~38 ℃
Odor
Slight typical rubber product odor
Specific Gravity
1.3-1.6
Decomposition Temperature
>250 ℃